Seam — where it appears
Named by 7 essays across 2 fields — each of them below, with the objects they name alongside it.
What holds a thread in a seam
A seam fails in two quite different ways, and the one the trade worries about is not the stitches breaking. It is the cloth's own threads sliding out of the weave beside the seam — and what resists that is friction at the crossings, accumulating multiplicatively, so a satin gives a seam a thousandth of the grip a plain weave gives it.
The stitch that weakens the seam
More stitches per centimetre put more sewing thread across a seam and more holes through the cloth beside it, so seam strength rises, crosses and falls. Whether the fabric line falls at all is decided by the clear gap between two threads against the width of the needle — the same arithmetic a filter cloth is specified by, doing a different job.
A seam slips before it breaks
A sewn seam fails in one of two ways and the trade names them separately: the threads pull out of the cloth beside the stitching, or something breaks. Which one a given cloth does is decided by whether its seam allowance clears the length at which grip beats strength — and at the ordinary ten millimetres, the table divides four against four.
A garment is cut dry and worn wet
A cutting allowance is one number and the thing it allows for is two, in two directions. Worse: when the two directions differ, a panel cut on the bias does not merely shrink — it rotates, by half a degree for an ordinary poplin, which is nine and a half millimetres of skew across a metre and is invisible to a tape measure.
A sewing thread is a different animal
It is folded, balanced, lubricated and finished, and every one of those is an answer to a requirement no weaving yarn has. The lubricant is the interesting one: it makes the thread sewable by lowering the friction that was holding its own fibres together.
A seam stands proud and wears first
A seam allowance is three plies where the garment is one, so it stands three quarters of a millimetre above a cloth whose own surface has a few micrometres of contact in it. Anything flat rubbed across the garment touches the seam and nothing else — all of the wear on two or three per cent of the area, until a whole thickness of fabric has been crushed.
A crease cannot cross a seam
The outer layer of a folded stack has further to go than the inner, by the fold's angle times the stack's own thickness. A four-layer seam of quarter-millimetre cloth taken through a half turn needs its outer layer to be 2.45 millimetres longer than its inner — and a stitch line every three millimetres has pinned them. So the fold opens out where it crosses the seam, which is what a trouser crease visibly does, and the arithmetic gives the radius it opens to.
Named alongside it
The objects these essays reach for when they reach for this one.
FrictionSeam slippageSpecificationAbrasionCloth thicknessFloatSettAllowanceAnchorageBearing curveBiasCalendering