Named by 7 essays across 2 fields — each of them below, with the objects they name alongside it.
A crease is a fold the crimp cannot supply
A fold needs its outer face longer than its inner, and a woven cloth's way of supplying a length is to move crimp. That runs out at a radius of millimetres, and a pressed crease is tenths of one — so the fold is handed to the fibres. How hard it strains them turns on a question this collection has been unable to settle for two fields, and a crease settles it by refusing.
Which fibres crease, and why there are two answers
Run the sharpest fold a yarn can make against every fibre's breaking extension and its recovery, and the ranking that falls out is the trade's own — linen worst, cotton next, wool and the melt-spun filaments best. It falls out of two columns rather than one, because two fibres in the bottom three get there by different mechanisms, and a treatment that fixes one does nothing for the other.
What a loop presses with
A knitted loop hangs on the loop below it and presses on it with a force nobody has been able to state. Solved from the loop's own bending it comes to about forty millinewtons a stitch — an order of magnitude under a woven crossing's, by two independent routes that have nothing in common.
The modulus a knit has instead of one
A fabric's stiffness in extension is usually its yarn's modulus with the geometry taken out. A knit's is not: dimensionally it can only be a bending rigidity over a length cubed, and the same yarn laid straight and parallel is thirty thousand times stiffer than the fabric made of it.
A knit bends more easily along its courses
A jersey is not a soft fabric to bend. Computed the same way as this collection's woven cloths it lands inside their band, at the limp end — and the useful number is not the magnitude but the direction: two point two to one between its two axes, with the soft one being the axis it rolls about.
What leaving the plane costs
Every number the flat loop model produced, beside the same number with the climb in it. Four of the five fall, none moves by four per cent, and the estimate that priced the third dimension beforehand had the sign the wrong way round for a reason worth naming.
A wrinkle cannot settle what a crease settles
The first rung of this ladder found that a pressed crease decides a question this collection had been unable to settle for two fields — whether a bent yarn's fibres slide or bend as one body — and it decides it by refusing: the coherent branch would strain the fibres by eighty-four per cent and cotton breaks at six. A wrinkle is the same fold at twenty times the radius, and there both branches are survivable. So the bracket that a crease collapses stays fourteen times wide at every radius anybody actually creases a cloth at accidentally.