Two pore systems in one cloth — 24 threads per centimetre
A plain weave of 20 tex cotton in section, at 24 threads per centimetre, so the yarn is 167 µm across and the clear hole between two picks is 250 µm. That hole's hydraulic radius is 124.8 µm. Inside the yarn, fibres 14 µm across packed at 0.6 leave spaces of hydraulic radius 2.33 µm — 53 times finer, and by Jurin's law 53 times higher: 6.37 m against 119 mm. The yarn's interior is magnified 6 times and the two discs at the foot are the only part drawn at one scale.
4 essays call
wick-section. The drawing above is what it returns with no arguments at all; every
call below passes it something, because a placement that passes nothing draws whichever
member of the family the generator happens to default to rather than the weave its essay
argues about.
Where it is called
Every figure listed here is drawn from this one rule.
The sett decides how much, not how high
Every essay on wicking so far has found the sett deciding something. This one finds it deciding nothing at all: a cloth's maximum rise is 6.37 m at eight threads per centimetre and 6.37 m at thirty-four, because the sett cannot reach inside a yarn.
How high a cloth wicks
A woven cloth has two capillary systems and they are a factor of twenty to a hundred apart. The one every diagram draws — the hole between four threads — lifts 119 mm. The one nobody draws, inside the yarn, lifts 6.37 m.
Wicking is slower along a crimped thread
A front travelling up a warp end travels the thread's path, which is longer than the cloth by exactly the crimp. So the wicking coefficient measured on the fabric is the yarn's own divided by (1 + c)² — 14.3 per cent lost at eight per cent crimp, whatever the liquid.
A drying cloth cannot lift what a sealed tube can
Every rise on this account is an equilibrium in a sealed tube, and a garment is neither sealed nor at equilibrium. Balancing the supply up a strip against the loss from its faces gives a quadratic whose width cancels exactly: in an ordinary room the fine system between the fibres stands at 500 millimetres instead of 6.37 metres, keeping 7.9 per cent of what a tube would give it, while the coarse system loses a third of a per cent. The forty-sixfold advantage becomes 3.7, and in a drying wind it reverses.